Gnee Steel (Tianjin) Co., Ltd.

Copper Alloy Extrusion Temperature Ranges and Process Control

Mar 27, 2024

What Sets the Copper Alloy Extrusion Temperature Window

Copper and copper alloys extrude reliably only inside a narrow thermal band. The billet must be hot enough to cut deformation resistance and restore plasticity, yet cool enough to avoid overheating, overburning and heavy surface oxidation. For any given grade the working range is derived from three references: the plasticity diagram, the recrystallisation diagram and the phase diagram, then trimmed to the real press line, die geometry and lubrication conditions.

The practical starting point is 0.75 to 0.95 times the melting point of the alloy. The upper limit of the range follows from the melting point of the metal, the solidus temperature on the phase diagram and the risk of hot brittleness in the form of overheating and overburning. The lower limit follows from the need for good plasticity at temperature and from available press capacity, because a cooler billet multiplies the force required to push metal through the die.

Selection Rules for Hot Extrusion of Copper Alloys

Stay in the single-phase region. Alloys that undergo a phase change at high temperature are best hot extruded in the single-phase field, so the billet flows uniformly instead of tearing along a duplex structure.

Avoid transverse cracking. Extrude inside the high-temperature plastic zone as far as possible, and at the same time watch surface behaviour, since excessive oxidation or sticking of the ingot skin to the tool destroys both finish and yield.

Respect temperature-dependent adhesion. Certain alloys grow more adhesive to tooling as they get hotter, which is typical of white copper and aluminium bronze. Run these grades as cool as the press allows and support them with adequate lubrication.

Match press capacity to temperature. Lower extrusion temperatures demand large-tonnage presses, because the same section requires far higher pressure at a cooler billet temperature.

Allow for deformation heat. Extrusion elbows deform heavily and the deformation speed is high, so friction between metal and tool generates a large amount of heat and raises billet temperature during the pass. The furnace set point is therefore usually taken at the lower limit of the working range.

Start from the property target. Different mechanical properties are obtained by extruding at different temperatures, so the required temper, grain size and strength of the finished product must be fixed before the heating curve is chosen.

Typical Extrusion Practice by Alloy Family

Alloy family Typical designation Extrusion practice
Oxygen-free and ETP copper C10100, C10200, C11000 Hot extrusion in the high-plasticity range; a clean billet surface is essential to avoid skin defects
Phosphorus-deoxidised copper C12200 Practice close to ETP copper; extruded shells feed water tube production to ASTM B88 and EN 1057
Free-cutting brass HPb59-1 Higher heating temperature lengthens the tail shrinkage and increases pressure residue, so discard control matters
Two-phase brass H62, H68 Extruding too cold forms strip-like laps at the end of the extruded product
Aluminium bronze QAl9-4 type Adhesive to tooling at high temperature; extrude cool with generous lubrication
Cupronickel and white copper C70600, C71500 Lower temperature practice limits sticking to the container liner and die

Grade designations follow the applicable national or international system, for example GB/T 5231 for wrought copper and copper alloy grades and ASTM B111 for seamless condenser and heat exchanger tube stock. The composition behind a designation, not the label alone, decides the heating range, so the same family name can cover quite different practice.

Tooling, Lubrication and Billet Condition

The shape and wall thickness of the extruded product, the degree of deformation, the tool temperature and the lubrication conditions all have a measurable influence on the temperature that is really needed at the die. Thin, complex sections produced at high extrusion ratio generate more frictional heat yet lose temperature faster in the die land, so the billet is frequently charged slightly hotter while the container is preheated to flatten the thermal gradient across the billet section. Surface condition matters as much as temperature: oxide scale, casting skin and lubricant residue all convert into surface defects once the metal begins to flow.

When a plant targets tight dimensional tolerance and a stable grain structure, the sequence is normally fixed first and verified by trial afterwards: define the alloy window from the diagrams, pick the low end of the range that the press can still drive, control deformation heat through ram speed and lubrication, and measure exit temperature rather than trusting the furnace reading alone.

Frequently Asked Questions

Q: What is the basic rule for copper alloy extrusion temperature?
The heating temperature is generally set at 0.75 to 0.95 times the melting point of the alloy, then adjusted for plasticity, press capacity and surface requirements.

Q: Why should two-phase brass not be extruded too cold?
Grades such as H62 and H68 form strip-like laps at the end of the extruded product when the temperature is too low, which reduces yield and surface quality.

Q: Which copper alloys are extruded at the low end of the range?
White copper and aluminium bronze, because their adhesion to tooling rises with temperature, and they also need sufficient lubricant and press capacity.

Q: How does deformation heat affect the furnace set point?
Friction between the metal and the tool raises billet temperature during extrusion, so the heating temperature is usually chosen at the lower limit of the working range.

Q: Does extrusion temperature change mechanical properties?
Yes. Different extrusion temperatures produce different structures and mechanical properties, so the required properties should be defined before the heating temperature is selected.

Q: Why does press tonnage matter when setting temperature?
A lower extrusion temperature raises deformation resistance sharply, so a large-tonnage extruder is required to maintain output and section accuracy.

goTop