Grade Overview and the EN 1982 Basis
CuNi10Fe1Mn1-C is the casting grade of the 90/10 copper-nickel family, designated CC380H and specified in EN 1982, the European standard that covers copper and copper alloy ingots and castings. The trailing C in the name identifies it as a cast composition, distinguishing it from the wrought 90/10 grade that is supplied as tube, plate and bar under separate product standards.
EN 1982 provides the compositional framework and the route by which mechanical properties are agreed between purchaser and foundry, because the properties of a casting depend on the casting process, the section thickness and the soundness of the metal as much as on the alloy itself. The order should therefore state the grade, the casting process, the required inspection and the property level to be demonstrated.
Composition and Casting Behaviour
The alloy takes its name from its principal additions: approximately 10 % nickel, with iron and manganese at around 1 % each. The nickel content provides the corrosion resistance of the copper-nickel system, while iron improves resistance to flowing seawater and manganese supports the protective film and assists deoxidation during melting.
| Characteristic | Grade basis |
|---|---|
| Designation | CC380H, cast copper-nickel 90/10 |
| Governing standard | EN 1982, copper and copper alloy ingots and castings |
| Principal alloying elements | nickel about 10 %, iron and manganese about 1 % each |
| Wrought counterpart | CuNi10Fe1Mn (CW352H) for tube, plate and bar |
Copper-nickel melts require attention to gas content and cleanliness, since dissolved gas produces porosity that both weakens the casting and provides sites for corrosion initiation in seawater. Foundries therefore control melting practice, deoxidation and pouring temperature closely, and they use risering and gating designed for the shrinkage characteristics of the alloy.
Corrosion and Seawater Performance
The 90/10 copper-nickel system is one of the established answers to seawater service. The alloy forms an adherent, slowly growing surface film that limits further attack, and the iron addition is particularly important because it strengthens that film in fast-flowing seawater. The result is an alloy that resists general corrosion, erosion-corrosion and the attachment of marine organisms better than plain copper or bronze in comparable duty.
Two practical conditions still require design attention. Stagnant or sulphide-polluted water can damage the protective film, and high local velocities with entrained sand or air bubbles will erode it. Both are addressed by system design - flow control, filtration and avoiding dead legs - rather than by changing the alloy alone.
Mechanical Properties and Testing
Mechanical requirements for castings are agreed with the foundry against EN 1982, with tensile strength for the 90/10 cast family typically falling in the region of 300 to 400 MPa depending on process and section. Separately cast test pieces, or test pieces cut from a prolongation, are used to demonstrate the agreed values.
Non-destructive examination is commonly specified for seawater components. Radiography or dye penetrant inspection reveals internal and surface discontinuities, pressure testing proves containment on hollow parts, and a batch chemical analysis confirms the composition. The inspection regime should be set on the drawing, because the acceptable defect level depends on whether the part is a lightly stressed housing or a pressure-retaining component.
Applications and Supply
Typical applications are pump bodies and impellers, valve bodies and trim, seawater pipe fittings, heat exchanger water boxes, desalination plant components, propeller and shaft hardware, and other parts where a complex shape must survive continuous seawater contact. Sand casting and centrifugal casting are both used, and continuous casting can supply bar and tube shell for subsequent machining.
Suppliers of copper-nickel castings usually work from a drawing and a specification rather than from a stock list, so the enquiry should include the required grade and standard, the casting process, machining allowance, the inspection and test plan, and the documentation to be issued with the delivery.
Frequently Asked Questions
Q: What is CuNi10Fe1Mn1-C?
A: It is the cast 90/10 copper-nickel grade designated CC380H in EN 1982, the standard covering copper and copper alloy ingots and castings.
Q: How does it differ from the wrought 90/10 copper-nickel grade?
A: The wrought grade, CuNi10Fe1Mn (CW352H), is supplied as tube, plate and bar under its own product standards, while the cast grade is produced to shape with properties that depend on the casting process and section.
Q: Why is iron added to copper-nickel?
A: Iron strengthens the protective surface film so that the alloy withstands flowing seawater better, which is the property that makes the 90/10 family suitable for marine duty.
Q: What inspection is normal for seawater castings?
A: Radiography or dye penetrant examination, pressure testing of hollow parts and chemical analysis of the heat are the usual requirements, with mechanical testing on separately cast or prolongation test pieces.
Q: What information is needed to place an order?
A: The grade and standard, the casting process, the drawing and machining allowance, the required mechanical properties, and the inspection and test plan, including the documentation to be supplied.