Gnee Steel (Tianjin) Co., Ltd.

CuSn11Pb2-B ( CB482K )

Jan 05, 2024

CuSn11Pb2-B ( CB482K )

CuSn11Pb2-B ( CB482K )CuSn11Pb2-B ( CB482K )CuSn11Pb2-B ( CB482K )

 

Grade : CuSn11Pb2-B
Number: CB482K
Classification: Copper-tin alloy
Standard: EN 1982: 2008 Copper and copper alloys. Ingots and castings
Equivalent grades: Go here

 



Chemical composition % of grade CuSn11Pb2-B ( CB482K )

A suffix -B is added to the designation to identify material in the form of ingots
Fe Si Mn Ni P S Al Cu Pb Zn Sb Sn
max 0.15 max 0.01 max 0.2 max 2 max 0.05 max 0.08 max 0.01 83.5 - 86.5 0.7 - 2.5 max 2 max 0.2 10.7 - 12.5



Mechanical properties of grade CuSn11Pb2-B ( CB482K )

 

Rm - Tensile strength (MPa) (GS) 240
Rm - Tensile strength (MPa) (GZ) or (GC) 280

 

Rp0.2 0.2% proof strength (MPa) (GS) 130
Rp0.2 0.2% proof strength (MPa) (GZ) or (GC) 150

 

A - Min. elongation at fracture (%) (GS) or (GZ) or (GC) 5

 

Brinell hardness (HBW): (GS) 80
Brinell hardness (HBW): (GZ) or (GC) 90



Equivalent grades of grade CuSn11Pb2-B ( CB482K )

Warning! Only for reference

EU
EN
Germany
DIN,WNr
CuSn11Pb2-B
2.1065
GB-CuSn12Pb

 



Casting process

GS Sand casting
GM Permanent mould casting
GZ Centrifugal casting
GC Continuous casting
GP Pressure die casting



Material conditions

R Material condition designated by the minimum value of tensile strength requirement for the product with mandatory tensile strength and elongation requirements
H Material condition designated by the minimum value of hardness requirement for the product with mandatory hardness requirements



Mechanical properties

ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
 

CuSn11Pb2-B ( CB482K ) Copper-tin alloy
Chemical composition. Equivalents of CuSn11Pb2-B ( CB482K ).
Standards.1 Mechanical Properties. Hardness