Gnee Steel (Tianjin) Co., Ltd.

CuZn20Al2As ( CW702R )

Jan 12, 2024

CuZn20Al2As ( CW702R )

CuZn20Al2As ( CW702R )CuZn20Al2As ( CW702R )CuZn20Al2As ( CW702R )

Grade : CuZn20Al2As
Number: CW702R
Classification: Cupper alloy
Density 8.4 g/cm ³
Standard: EN 1653: 1998 Copper and copper alloys. Plate, sheet and circles for boilers, pressure vessels and hot water storage units
EN 12451: 1999 Copper and copper alloys. Seamless, round tubes for heat exchangers
EN 12452: 1999 Copper and copper alloys. Rolled, finned, seamless tubes for heat exchangers
EN 12449: 1999 Copper and copper alloys. Seamless, round tubes for general purposes
EN 1652: 1998 Copper and copper alloys. Plate, sheet, strip and circles for general purposes
Equivalent grades: Go here

 



Chemical composition % of grade CuZn20Al2As ( CW702R )

Fe Mn Ni P Al Cu As Pb Others -
max 0.07 max 0.1 max 0.1 max 0.01 1.8 - 2.3 76 - 79 0.02 - 0.06 max 0.05 total 0.3 Zn - remainder



Mechanical properties of grade CuZn20Al2As ( CW702R )

 

Rm - Tensile strength (MPa) (R330) 330
Rm - Tensile strength (MPa) (R390) 390

 

Rp0.2 0.2% proof strength (MPa) (R330) 90
Rp0.2 0.2% proof strength (MPa) (R390) 240

 

A - Min. elongation at fracture (%) (R330) 30
A - Min. elongation at fracture (%) (R390) 25

 

Vickers hardness ( HV): (H070) 70 - 105
Vickers hardness ( HV): (H100) 100



Properties CuZn20Al2As

This alloy may be used for sea water application



Equivalent grades of grade CuZn20Al2As ( CW702R )

Warning! Only for reference

EU
EN
Germany
DIN,WNr
CuZn20Al2As
2.0460
CuZn20Al2

 



Casting process

GS Sand casting
GM Permanent mould casting
GZ Centrifugal casting
GC Continuous casting
GP Pressure die casting



Material conditions

R Material condition designated by the minimum value of tensile strength requirement for the product with mandatory tensile strength and elongation requirements
H Material condition designated by the minimum value of hardness requirement for the product with mandatory hardness requirements



Mechanical properties

ReH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d elasticite minimale
Rm Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
 

CuZn20Al2As ( CW702R ) Cupper alloy
Chemical composition. Equivalents of CuZn20Al2As ( CW702R ).
Standards.1 Mechanical Properties. Hardness

goTop