What a Coating Must Do on Titanium
Titanium resists corrosion through a passive oxide film, but the same film makes the metal prone to galling and to adhesive wear, and it does not protect against high temperature oxidation. Engineering coatings are applied for three reasons: to reduce friction and wear, to extend service temperature beyond the roughly 500 °C at which oxide growth becomes rapid, and to provide a barrier in chloride or acid environments where the natural film is stressed.
Weight and strength are preserved because the coating is only a few micrometres to a few hundred micrometres thick, so a titanium part replaced by a coated titanium part does not surrender the 40% mass advantage it holds over steel.
Surface Preparation Before Any Coating
Adhesion on titanium is decided before the coating chamber is closed. Scale and oxygen-enriched surface layers are removed by blasting, machining or pickling, following practice such as ASTM B600 for descaling and cleaning titanium. The surface is then degreased, activated and kept free of iron contamination from steel brushes, racks or tooling, because embedded iron forms galvanic cells that undermine the layer in service.
For medical and implant components, preparation and cleaning follow ASTM F86, which defines the sequence of passivation and handling required so that the surface is not degraded after the final treatment. Components are dried and transferred to the coating operation without fingerprints, since a contaminated surface produces localised blistering rather than a uniform layer.
Coating Families and Where Each Fits
| Family | Typical thickness | Function |
|---|---|---|
| Anodic oxide | 1 – 30 µm | Wear resistance, colour coding, mild corrosion barrier |
| PVD nitride layers | 1 – 5 µm | Hard wear surface on tooling and fasteners |
| Thermal spray carbides and oxides | 50 – 500 µm | Abrasion resistance and thermal barrier on large parts |
| Plasma electrolytic oxide | 5 – 40 µm | Hard ceramic layer for high load contact |
Anodising is controlled through the electrolyte, current density and time, and layer condition is specified under AMS 2488, which defines the coating types and the acceptance tests rather than a single fixed thickness. Nitride layers deposited by physical vapour deposition reach microhardnesses in the range of 2000 to 3200 HV depending on the composition, and thermally sprayed carbide layers typically give 1000 to 1300 HV at much greater thickness, which suits parts that must resist coarse abrasion rather than fine sliding wear.
Process Windows and Adhesion Control
Deposition temperature is held below the level at which oxygen and nitrogen uptake becomes significant, or the procedure provides for removal of the affected layer afterwards.
Vacuum quality and target cleanliness are monitored, because residual oxygen in the chamber shifts the stoichiometry of a nitride layer.
Substrate bias and ion etching before deposition improve adhesion more reliably than increasing coating thickness.
Sharp edges and deep blind holes distort the thickness distribution and are best radiused or masked before treatment.
Hydrogen uptake is minimised by keeping acid exposure short and by avoiding any pickling step that generates free hydrogen on a high strength part.
Inspection and Acceptance Criteria
Layer thickness is verified by a calibrated magnetic or eddy current gauge on a coated coupon from the same run, backed by cross-section measurement. Adhesion is checked by bend, scratch or indentation methods appropriate to the layer, and hardness is confirmed by microhardness testing on a polished section. Corrosion performance where required is demonstrated by neutral salt spray to ISO 9227, and a visual check confirms colour and coverage consistency, especially on anodised parts where colour is a function of layer thickness.
The recurring mistake is to judge a coating by its appearance alone. A bright, uniform colour can hide a layer that is too thin to protect, and a thick layer can be porous and detach under load. Both conditions are detected by measurement, not by eye.
Frequently Asked Questions
Q: Which coating is used for coloured titanium fasteners?
A: An anodic oxide layer a few micrometres thick, applied so that light interference produces the colour. Layer condition is specified under AMS 2488.
Q: Can titanium be coated without losing its weight advantage?
A: Yes. Engineering coatings range from 1 to 500 micrometres depending on the family, so the mass increase is small compared with the strength and stiffness of the base part.
Q: Why is coating temperature limited?
A: Titanium absorbs oxygen, nitrogen and hydrogen aggressively above roughly 500 °C, which embrittles the surface and can reduce fatigue life.
Q: How is coating adhesion verified?
A: By bend, scratch or indentation tests on coated coupons from the same batch, supported by microhardness and layer thickness measurement on a cross section.
Q: Does a coating replace the natural passive film?
A: It supplements it. The engineered layer carries the wear or thermal duty, while the titanium oxide film continues to provide the corrosion barrier underneath.