GB Copper and Copper Alloy Designation Rules: T, H, Q and B Grade Codes

May 14, 2024

How the GB Copper Designation System Works

The Chinese national system for designating wrought copper and copper alloys, standardised in GB/T 5231, is built so that a compact code carries the whole alloy identity. The first capital letter is the pinyin initial of the Chinese family name: T for Tong (pure copper), H for Huangtong (brass, a copper-zinc alloy), Q for Qingtong (bronze) and B for Baitong (cupronickel, a copper-nickel alloy). Everything that follows the family letter describes composition - either the copper content in percent, or the symbol and nominal content of the alloying element that defines the grade. Product form, temper and dimensions are never encoded in the grade itself; they are stated separately in the product standard and the purchase order.

The Four Family Prefixes at a Glance

Type code Alloy family Pinyin source Typical designations
T Pure copper, including oxygen-free and deoxidised grades Tong T1, T2, T3, TU1, TU2, TP1, TP2
H Brass (copper-zinc) Huangtong H90, H68, H62, HPb59-1, HSn62-1, HAl77-2
Q Bronze (copper-tin and related alloys) Qingtong QSn6.5-0.1, QAl9-4, QBe2
B Cupronickel, also called white copper (copper-nickel) Baitong B19, B30, BFe30-1-1

Naming Rules Inside Each Family

Pure copper (T). The letter T is followed by a sequence number that reflects refining order and permitted impurity level: T1 is the highest-purity wrought grade, followed by T2 and T3. T2, with a minimum copper content of 99.90%, is the general-purpose grade and is comparable in composition to electrolytic tough pitch copper C11000. Two sub-families add a second letter. TU grades (TU1, TU2) are oxygen-free copper with a maximum oxygen content in the region of 0.002 to 0.003%, used where ductility after high-temperature brazing matters. TP grades (TP1, TP2) are phosphorus-deoxidised copper with residual phosphorus of roughly 0.005 to 0.050%; TP2 corresponds closely to C12200, the classic copper for water and refrigeration tube.

Brass (H). Binary copper-zinc brasses carry the nominal copper content in percent: H90 at 88.0 to 91.0% Cu, H68 at 67.0 to 70.0% Cu and H62 at 60.5 to 63.5% Cu. When a third element defines the grade, its chemical symbol and nominal content are inserted before the copper figure, which is why HPb59-1 describes a leaded brass with about 59% Cu and 1% Pb, and HSn62-1 a tin brass. In this family the number before the hyphen is copper and the number after it is the alloying addition.

Bronze (Q). Bronze designations follow the pattern Q + element + content directly, because properties are governed by the alloying element rather than by a copper minimum. Examples are QSn6.5-0.1 (about 6.5% Sn with 0.1% P) for spring and bearing strip, QAl9-4 (about 9% Al with 4% Fe) for wear-resistant parts and QBe2 (about 2% Be) for high-strength electrical springs. Where two figures appear, the second is a property-modifying addition whose permitted range is usually narrow.

Cupronickel (B). B grades state the nickel content: B19 contains about 19% Ni and B30 about 30% Ni. Complex grades add further symbols, as in BFe30-1-1, where roughly 30% Ni is combined with about 1% Fe and 1% Mn; the iron and manganese additions are what give the grade its resistance to fast-flowing seawater.

Reading a Designation Correctly and Cross-Referencing Other Systems

The leading letter is always the alloy family, never a temper or a product form.

For brass, the figure before the hyphen is the nominal copper content; for cupronickel, the figure is the nominal nickel content.

Figures after a hyphen give the nominal content of the named alloying element.

Temper (soft, quarter hard, half hard, hard) and product form are declared separately, for example in the sheet, tube or rod standard.

Casting alloys are designated under GB/T 1176 and carry a Z prefix, so the wrought naming rules above must not be applied to castings.

Cross-referencing to ASTM, EN or UNS numbers is useful but never exact. A sound practice is to compare composition ranges and temper rather than short codes alone. T2 is normally matched with C11000, TP2 with C12200 and TU1 with C10100 or C10200; H68 is compared with C26000, H65 with C27000, H62 with C27400 or C28000, HSn70-1 with C44300 and BFe30-1-1 with C71500. Impurity limits, residual element allowances and mechanical ranges still differ between GB/T 5231 and the corresponding foreign specification, so each order should be checked against the actual standard text.

Procurement Notes: Turning a Grade Code Into a Verifiable Order

Three details decide whether a GB-grade enquiry is met exactly. First, quote the standard and its year of issue, because grade ranges and tolerances are revised over time and a bare grade such as H62 on a drawing is not a complete specification. Second, name the product form and its own standard, since sheet, strip, tube, rod and wire each have separate dimensional and mechanical requirements. Third, state the temper and the acceptance test, such as tensile strength, elongation or annealed grain size, so that supplier and buyer measure the same property. Together these three items convert a short GB code into a purchase order that can be inspected and verified on delivery.

Frequently Asked Questions

Q: What do the letters T, H, Q and B mean in GB copper designations?
T stands for pure copper, H for brass, Q for bronze and B for cupronickel. Each letter is the pinyin initial of the Chinese family name, so the first character already tells the buyer which alloy system the grade belongs to.

Q: How can I tell copper content from a designation such as H62 or HPb59-1?
In the brass family the figure before the hyphen is the nominal copper content, so H62 contains about 62% Cu. In HPb59-1 the same 59 refers to copper, while the 1 after the hyphen is the nominal lead content.

Q: What is the difference between T2, TU2 and TP2?
T2 is electrolytic tough pitch copper with at least 99.90% Cu. TU2 is oxygen-free copper with oxygen limited to a few thousandths of a percent, and TP2 is phosphorus-deoxidised copper containing a controlled residual of about 0.01 to 0.05% P. The choice depends on whether brazing ductility or weldability in a reducing atmosphere matters most.

Q: Does a GB grade convert directly to an ASTM or UNS grade?
No. The nearest UNS grade is a useful starting point for comparison, but composition ranges, impurity limits and mechanical requirements are set independently by each standard, so equivalence must be confirmed against the specific product specification.

Q: Is the same naming system used for cast copper alloys?
No. Wrought products are designated under GB/T 5231, while casting alloys follow GB/T 1176 and use a Z prefix. Designations from the two systems should never be substituted for one another.

Q: What information should be added to a grade code on a purchase order?
The standard number with its year, the product form and its dimensional standard, the temper, and the acceptance tests with their limits. A grade code alone does not define a deliverable product.