Material Designation and Chemistry of H68 Brass
H68 is a single-phase alpha brass standardised in GB/T 5231. It is the most formable of the common brasses because its zinc content stays below the point at which a second phase appears, so the microstructure remains uniform and the sheet or strip can be cold reduced and deep drawn to a high degree without cracking. The designation is the Chinese GB grade; the nearest equivalents elsewhere are UNS C26200, EN CuZn30 and the JIS C2600 class.
| Element | Limit (%) |
|---|---|
| Cu | 67.0-70.0 |
| Pb | 0.03 max |
| Fe | 0.10 max |
| Sb | 0.005 max |
| Bi | 0.002 max |
| Total impurities | 0.30 max |
| Zn | Balance |
The tightly controlled lead, antimony and bismuth limits exist because those elements are harmful to hot ductility at the levels found in free-cutting brasses. That is why H68 is specified as a cold-forming material rather than as a machining grade.
Properties of H68 Brass
Plasticity: the best among the common brasses, with excellent cold deep drawing, stamping, spinning and bending behaviour.
Strength: tensile strength of at least 370 MPa in the half-hard temper, rising in harder tempers, which is adequate for light structural parts.
Joining: easy brazing and soldering, and welding can be carried out with appropriate care.
Corrosion resistance: good in ordinary atmospheres and in fresh water.
Stress-corrosion risk: residual stress can produce season cracking in ammoniacal or humid environments, so a stress-relief anneal follows cold work whenever a formed part will see that service.
Machinability: good, though lower than in the leaded free-cutting brasses, because the lead content is restricted to 0.03% maximum.
The combination of high plasticity and moderate strength is what makes the grade useful: parts can be formed in a single press stroke where a harder brass would need an intermediate anneal, and the finished component still carries a working load.
Heat Treatment Schedule
| Operation | Temperature (C) | Purpose |
|---|---|---|
| Hot working | 750-830 | Hot forming range for the alloy |
| Annealing, softening | 520-650 | Restores ductility after cold reduction |
| Stress-relief annealing | 260-270 | Removes residual stress to prevent season cracking |
The three rows describe three different intentions and should not be confused with each other. Softening anneal is applied between cold-forming steps when the material has exhausted its ductility and must be recrystallised. Stress-relief annealing is applied after the last forming operation and is deliberately kept below the recrystallisation range: it relaxes the locked-in stress that drives season cracking, yet it leaves the cold-worked strength and the dimensional accuracy of the finished part intact. Raising a stress-relief treatment into the softening range would undo the work hardening that the part depends on.
Applications of H68 Brass
The grade is used for deep-drawn and bent parts, including pins, rivets, washers, nuts, conduits and tubing, pressure-gauge springs, screens and mesh, radiator fins and tubes, cartridge cases, and general hardware and decorative items. Three themes run through that list. First, a severe forming operation in which the metal must flow without tearing. Second, a need for a smooth, corrosion-resistant surface that can be polished or plated. Third, a requirement for good thermal or electrical behaviour in a part that is also formed, as in radiator tubes and gauge springs.
Where a part combines deep drawing with subsequent soldering or brazing, the low impurity limits of H68 pay off again, because the alloy tolerates the thermal cycle of joining without the cracking that a leaded brass can suffer.
Supply Forms and Certification
| Product form | Standard |
|---|---|
| Sheet and strip | GB/T 2040 |
| Tube | GB/T 1527 |
| Rod | GB/T 4423 |
| Wire | Available in drawn form for forming and mesh |
| Certification | EN 10204 3.1 inspection certificate |
| Condition options | Soft, half-hard and harder tempers, with stress-relief option for formed parts |
For formed parts the ordering specification should state the temper and whether a stress-relief anneal is required after forming. That single sentence determines whether a deep-drawn component survives a humid or ammoniacal service environment, and it is far cheaper to specify before the tools are built than to rectify afterwards.
Frequently Asked Questions
Q: What is H68 brass?
H68 is a single-phase alpha brass standardised in GB/T 5231, with 67.0-70.0% copper, lead limited to 0.03% maximum and zinc as the balance, equivalent to UNS C26200 and EN CuZn30.
Q: Why is H68 considered the most formable common brass?
Its zinc content stays below the level that creates a second phase, so the structure remains uniform and the strip can be deep drawn, spun and bent without cracking.
Q: What are the heat treatment temperatures for H68?
Hot working at 750-830 C, softening anneal at 520-650 C, and stress-relief annealing at 260-270 C after cold working.
Q: Does H68 brass suffer stress-corrosion cracking?
It can. Residual stress in a cold-worked part can lead to season cracking in ammoniacal or humid conditions, which is why stress-relief annealing at 260-270 C is recommended.
Q: What is the strength of H68 brass?
Tensile strength is at least 370 MPa in the half-hard temper, and it rises further in the harder tempers for light structural applications.
Q: Which products are made from H68 brass?
Deep-drawn and bent parts such as pins, rivets, washers, nuts, conduits and tubing, gauge springs, screens and mesh, radiator fins and tubes, cartridge cases and decorative hardware.
Q: How are H68 sheet, tube and rod supplied?
Sheet and strip to GB/T 2040, tube to GB/T 1527 and rod to GB/T 4423, with an EN 10204 3.1 certificate and a stress-relief option for formed parts.