Detailed analysis of the causes of casting cracks in copper castings



1. Cracking resistance of copper castings
Hot cracking of an alloy refers to the tendency of the alloy to form cracks at high temperatures. It is one of the common casting defects of some copper alloy castings. Usually the shape of hot cracks is tortuous and irregular, occurring along grain boundaries. The surface of the crack is often strongly oxidized and has no metallic luster.
According to its position on the casting, hot cracking is often divided into external cracking and internal cracking. External cracks often start from casting surface irregularities, sharp corners, changes in cross-section thickness, and other similar places that can produce stress concentrations. Gradually extends into the interior of the casting, with a wider surface and a narrower interior, and sometimes runs through the entire casting section. Internal cracks occur at the final solidification point inside the casting. Generally does not extend to the surface of the casting. The surface of the crack is very uneven, often with many forks, and the degree of oxidation is lighter than that of the outer crack.
It is generally believed that hot cracking of alloys occurs during the solidification process, that is, when most of the alloy has solidified, but there is still a small amount of liquid between the dendrites. At this time, the linear shrinkage of the alloy is large and the strength of the alloy is low. If the casting mold prevents its shrinkage, the casting will produce a large shrinkage stress acting on the hot joint. When the strain at the hot joint is greater than the allowable strain of the alloy at that temperature, hot cracking will occur.
However, for the same alloy, whether hot cracking occurs in castings often depends on factors such as casting resistance, casting structure, and pouring process. During the condensation process of castings, any method that can reduce its shrinkage stress and improve the high-temperature strength of the alloy will help prevent the occurrence of hot cracks. Therefore, in actual production, effective measures such as increasing the yieldability of the casting mold, improving the mold structure, improving the location where the alloy is introduced into the casting mold, and rationally setting reinforcement ribs and cooling are usually taken to avoid hot cracking. The tendency of the alloy to hot crack depends on the properties of the alloy. Generally speaking, the greater the difference between the temperature at which a complete dendrite skeleton begins to form during the solidification process of the alloy and the temperature at which the solidification ends, and the greater the shrinkage rate of the alloy during this period, the greater the difference. The greater the tendency of the alloy to be thermally cracked.
2. Pressure resistance
Poor pressure resistance of castings means that when pressure is applied to die castings, pressure leaks from the inside or outside of the castings, which may manifest as oil leakage, air leakage, water leakage, etc. It is one of the most difficult problems to solve among casting defects, and the causes may be various. Defects caused by the combination of defects.
The casting is immersed in water, and the inner cavity of the casting is filled with compressed air. The compressed air passes through the path formed by the inner surface defects, internal defects and outer surface defects of the casting and reaches the water surface. Bubbles appear, indicating poor pressure inspection.
In copper alloy castings, the requirements for alloy density are high, so improving the hydraulic resistance of copper alloy castings and avoiding leakage have become the key to production. It has been verified by production that as long as a certain thickness of columnar crystals or fine equiaxed crystal structures is obtained in the cross section of the casting, the hydraulic pressure resistance can meet the usage requirements. However, columnar crystals are easy to obtain under rapid cooling conditions, but are difficult to obtain under general sand casting conditions. For specific castings, the method of increasing the pouring temperature to obtain a columnar crystal structure has a very obvious effect. The pouring temperature of copper castings is too low, the alloy structure is loose, the leakage problem of castings is serious, and "tin sweat" and hot cracking occur from time to time.
When the pouring temperature is increased, the casting structure becomes dense columnar crystals, and qualified castings are obtained. (Source: Copper Alloy Casting)