Gnee Steel (Tianjin) Co., Ltd.

Purple Copper Pipe Leaks and 100% Eddy Current Testing

Oct 07, 2023

What Purple Copper Pipe Is

Purple copper pipe is the trade name for the deep red phosphorus-deoxidised copper tube that dominates air conditioning and refrigeration work. In the Chinese designation system it is TP2, and it corresponds to the Cu-DHP grade of EN 1412, which is also known as UNS C12200. The residual phosphorus level of roughly 0.015 to 0.040 % deoxidises the melt, so the tube can be brazed and welded without the hydrogen embrittlement that affects oxygen-bearing copper.

Drawn tube of this type is produced to product standards such as GB/T 1527 for drawn copper and copper alloy tubes and to EN 12449 for seamless round copper tubes for general purposes. Refrigeration duty adds cleanliness, dryness and pressure-integrity requirements on top of the dimensional specification.

Where Leaks Originate in Production

Copper tube leakage is the failure mode that matters most to an air conditioning manufacturer, because loss of the refrigerant charge stops the system from transferring heat at all. The causes cluster in three groups. The first is tube-wall defects: laps, seams, inclusions and thin walls produced during casting and drawing. The second is mechanical damage introduced after drawing, such as scores, dents and crushing during coiling or handling. The third is joint quality at the customer's own brazing station, which is influenced by the ovality, cleanliness and dimensional consistency of the tube supplied.

Because the first two groups originate in the mill, they must be detected in the mill. That is why eddy current examination is the central quality gate in tube production rather than an optional extra test.

Eddy Current Testing and Full Coverage

Eddy current testing passes the tube through a coil that induces circulating currents in the wall. A discontinuity in the wall changes the impedance of the coil, and the instrument registers a signal proportional to the defect. On-line examination therefore inspects the entire length and the full circumference without contact and at production speed, and the practice is standardised in GB/T 5248 for copper and copper alloy tubes and in the EN 1971 series for the eddy current testing of seamless round copper and copper alloy tubes.

Products supplied for air conditioning and refrigeration are routinely released only after 100 % eddy current examination, which means every length produced has passed through the coil rather than a sampled portion of the order. Where an order also includes a hydrostatic or pneumatic pressure test, the two checks are complementary: the pressure test proves containment at the test pressure, while eddy current detects the small defects that may not open under that pressure.

Calibration with Artificial Defects

An eddy current result is only meaningful if the instrument sensitivity is anchored to a known reference. The usual practice is to calibrate the flaw detector on a reference tube carrying artificial defects of defined geometry, most often a drilled through-hole of specified diameter, and the acceptance threshold is then set as a percentage of the signal from that reference defect. This is what prevents the two opposite failures from occurring at the same time: excessive false rejection of sound tube, and the release of tube carrying defects that should have been caught.

Calibration is repeated at defined intervals and after any change of coil, tube size or settings, and the reference tube itself is controlled as a measuring instrument with its own records. Without this discipline the examination is a paper exercise rather than a control.

Defect Marking, Sorting and Process Control

When the instrument flags a defect, the location is marked - commonly with an ink mark or an automated paint spot - so that the affected section can be located, cut out and segregated. Rejected material is not reworked into a lower grade without a documented decision, because a defective tube released into a refrigeration circuit fails after the system is charged and installed, at far greater cost than the scrap value of the section.

Trend analysis of defect signals closes the loop. A rising rate of signal in one drawing line, one die or one casting batch points to a specific process problem, and correcting that source reduces leakage downstream. Suppliers who record examination data by heat, coil and drawing line convert a quality gate into a process improvement tool.

Frequently Asked Questions

Q: What is purple copper pipe called in the European system?

A: It is Cu-DHP in the designation system of EN 1412, equivalent to UNS C12200 and to TP2 in the Chinese system, a phosphorus-deoxidised copper with about 0.015 to 0.040 % phosphorus.

Q: Why is 100 % eddy current testing used instead of sampling?

A: A single through-wall defect can scrap an entire charged refrigeration system, so every length is examined on line rather than a sample of the order.

Q: How is the sensitivity of the examination established?

A: The instrument is calibrated on a reference tube containing an artificial defect such as a drilled through-hole of defined diameter, and the acceptance level is set against that signal.

Q: Does a pressure test replace eddy current examination?

A: No. A pressure test proves that the tube contains the test pressure, while eddy current examination detects small discontinuities that may not open at that pressure but can grow in service.

Q: What happens to tube that fails the examination?

A: The defective section is located by its mark, cut out and segregated under a documented disposition decision so that no defective length can enter a finished circuit.

goTop