S-Cu-8 (CS053B) Grade Overview
S-Cu-8, recorded under the number CS053B, is a copper alloy scrap grade published in EN 12861:1999, the European standard for copper and copper alloys in scrap form. It is the most tolerant of the three grades in this family: the copper minimum is 98 % including silver, oxygen is limited to 0.06 %, and the ceilings on iron, lead, zinc, tin, nickel and aluminium are an order of magnitude looser than those of the higher purity scrap categories. CS053B is therefore the grade a copper producer selects when the yield of the charge matters more than the conductivity of the finished product.
The grade is classified as copper alloy scrap and carries no listed equivalents, so its identity is confirmed by analysis. Its value in the melt shop comes from a composition that is wide enough to accept ordinary process scrap, yet still bounded, so that furnace practice and product quality remain predictable.
Chemical Composition of S-Cu-8 (CS053B)
Every figure is a maximum unless a minimum is stated. Silver is counted with the copper, oxygen is limited to 0.06 %, and the residual allowance for unlisted elements is expressed as a total rather than on an individual basis.
| Element | Limit, % | Effect on processing |
|---|---|---|
| Cu including Ag | min 98 | Base metal content |
| O | max 0.06 | Casting porosity and hydrogen sensitivity |
| Fe | max 0.3 | Raises strength, reduces conductivity |
| Ni | max 0.1 | Affects conductivity and colour |
| Al | max 0.05 | Oxide inclusions in the melt |
| Pb | max 0.5 | Hot-shortness during rolling and drawing |
| Zn | max 0.5 | Fume and zinc loss in the furnace |
| Sn | max 0.25 | Raises hardness and lowers ductility |
| Other elements | total 0.05 | Combined residual allowance |
Two features distinguish CS053B from the tighter grades. First, lead and zinc are allowed up to 0.5 % each, roughly ten times the ceiling found in high-purity copper scrap; both elements can be tolerated in alloys and in remelt products that do not need maximum conductivity, but both must be watched in the furnace, because zinc volatilises and lead segregates. Second, the unlisted residual allowance is a single 0.05 % total, which means several minor elements can be present at once provided their sum stays inside the limit.
Standard Basis and Designation Rules
EN 12861:1999 sets the designation, sampling and characterisation rules for copper and copper alloy scrap and fixes the chemical limits that define each grade. No equivalent grades are listed for S-Cu-8, so any replacement material has to be qualified against the composition table by agreed analysis. Because this grade accepts a comparatively wide chemistry, chemical confirmation matters more rather than less: a lot that passes a visual inspection can still exceed the zinc or lead ceiling once it is analysed.
Chemistry, not the trade description, establishes the grade of a delivered lot.
Samples must represent the entire consignment, since scrap lots are heterogeneous.
Mixed alloy, plated and soldered material, coatings, oil and moisture must be removed before charging.
Casting and Condition Designations Used with the Grade
The grade record also carries the standard letter codes for casting route and delivery condition used across copper alloy specifications. They describe production route and ordering condition without adding chemistry limits.
GS – sand casting
GM – permanent mould casting
GZ – centrifugal casting
GC – continuous casting
GP – pressure die casting
R – condition defined by a minimum tensile strength, with tensile strength and elongation mandatory
H – condition defined by a minimum hardness, with hardness mandatory
The property symbols ReH for minimum yield strength, Rm for tensile strength, A for minimum elongation and J for the notch impact test are listed alongside them. For a scrap grade none of these is a mandatory limit; they take contractual effect only when a cast product is ordered to a stated condition.
Inspection, Sampling and Melting Practice
Lots of CS053B are verified in the same two stages as other scrap grades. Physical sorting removes mixed alloy, soldered or plated material, insulation and moisture and prepares the lot for representative sampling; instrumental checking then follows, using X-ray fluorescence or spark analysis on prepared samples. The decisive step is the bath analysis taken after melting and before casting, because it is the only point at which the whole heat can be corrected or rejected. With lead and zinc permitted up to 0.5 % a piece, sorting discipline and a reliable bath analysis are what keep an off-analysis heat out of the caster.
In the melt shop the grade is charged to make wire rod, strip, castings and general copper products where a moderate iron, tin and nickel level is acceptable. Melting practice focuses on two risks: zinc volatilising from the melt, which changes the analysis and produces fume, and lead segregation, which shows up as cracking during hot working. Both are managed by controlling charge composition, melt temperature and holding time rather than by refining after the fact.
Frequently Asked Questions
Q: What is S-Cu-8 CS053B?
It is a copper alloy scrap grade defined in EN 12861:1999 with a minimum of 98 % copper including silver and limits of iron 0.3 %, nickel 0.1 %, aluminium 0.05 %, lead 0.5 %, zinc 0.5 % and tin 0.25 %.
Q: How does it differ from higher purity copper scrap grades?
The copper minimum is lower at 98 % and the ceilings on iron, lead, zinc and tin are far looser, so the grade is chosen for charge yield rather than for maximum conductivity.
Q: What does the total 0.05 % residual allowance mean?
It is a combined limit: minor unlisted elements may be present together provided their sum does not exceed 0.05 %.
Q: Which standard governs the grade?
EN 12861:1999, the European standard for copper and copper alloys in scrap form, which sets the designation and the chemical limits.
Q: Why does zinc need attention in the furnace?
Zinc is allowed up to 0.5 %, and because it volatilises at melting temperature it can change the bath analysis and generate fume, so melt temperature and holding time must be controlled.
Q: How is the composition of a lot confirmed?
Physical sorting and sampling are followed by X-ray fluorescence or spark analysis, and the heat is then confirmed by a bath analysis after melting and before casting.