How to weld water-stop copper strip

A 50-watt internal heating soldering iron, rosin solder wire, fine sandpaper, and needle-nosed pliers will suffice. Use sandpaper to remove the oxide layer on the surface of the water-stop copper tape until it is shiny. Heat an electric soldering iron to plating tin on each water-stop copper tape. Then the two copper sheets are overlapped together and melted by heating with the electric soldering iron.

Waterproof copper strip welding process test

There is no need to make the welded joint of the water-stop copper tape into a bull-nose shape, just two pieces can be welded on both sides. When the water-stop copper sheet is designed as a water-stop copper strip, the test piece should be sent for inspection according to the designed special shape according to the on-site supervision requirements. If there is no requirement for on-site supervision, the test piece can be submitted for inspection normally as usual.

Here, a brief introduction to the welding process and detection methods of water-stop copper strips:

1. Double-sided lap welding is used to connect the water-stop copper strips, and the lap length is not less than 20mm. Brass electrode gas welding should be used for welding, and manual arc welding should not be used.

2. Welding operating conditions: 1) Welders should be trained and assessed, hold a certificate to work, and be familiar with mechanical properties and operating procedures. 2) All gas welding equipment must be inspected before work or when working again after a long downtime. The joints and valve fasteners of acetylene bottles, oxygen bottles and rubber hoses should be tight and secure, and no looseness, damage or air leakage is allowed. Oxygen bottles and their accessories, rubber hoses and tools should not be contaminated with grease and dirt. In this way This ensures that no accidents will occur due to malfunction of the gas welding equipment during the gas welding process. 3) Check gas welding equipment, accessories and pipelines for leaks. Only use soapy water for testing. During the test, no open flames or smoking are allowed around to avoid causing fire. 4) The distance between oxygen bottles, acetylene bottles and open flames should be more than 10 meters. If conditions are extreme, it should not be lower than 5 meters, and isolation measures should be taken.

3. The welding method is to use oxygen and acetylene to generate high temperature, melt the metal of the welding rod and the weldment, and then solidify to form a weld.

4. In order to obtain high-quality welding joints, the shape and size of the welding pool should always be consistent.

5. Testing methods and test results should be inspected one by one according to the relevant provisions of GB/T528, and there should be no bubbles, slag inclusions or false welding. If necessary, conduct a strength check. The tensile strength should not be less than 75% of the strength of the base material. The welded joints should have a smooth surface, no holes, gaps, and no water seepage.

Copper waterstop welding

Test method for welding quality of copper water-stop copper strip water-stops

1. The copper waterstop welded joint can be inspected from the appearance quality

After the welding is completed, use visual inspection or measurement to check whether the weld is flat and smooth, whether the interface error of the axis time meets the technical requirements of the bidding document and the overlap length is not less than 20mm.

2. Kerosene penetration test of welded joints

First, clean the surface of the part for inspection without leaving any stains. Apply it with white powder slurry. After it is completely dry, apply kerosene on the back of the weld. Due to the tension effect of kerosene, it has the characteristic of penetrating into small gaps. If the welding seam of the copper water-stop sheet is not tight or there is looseness, interlayer, or dust inside the steel, the kerosene will leak from the copper water-stop sheet to the other side of the steel material or weld and show stains on the white powder.

In order to accurately determine the location of the defect and avoid the spread of the print stain, stop for a moment after applying kerosene and observe. The location where the print stain first appears is the location of the defect. In order to ensure that the kerosene has sufficient infiltration time, it is appropriate to ensure that the detection process lasts for more than half an hour without any stains.

3. Mechanical property testing methods of welded joints

The joint tensile test should not be less than 80% of the tensile strength of the base material. This area needs to be strictly controlled.

How to weld copper sheets to copper sheets

Before using a new soldering iron, polish the tip with fine sandpaper, apply electricity and heat it, dip it in rosin and touch the blade edge of the tip to the soldering wire to evenly coat the tip with tin. Doing so can facilitate welding and prevent the surface of the soldering iron tip from oxidizing. If the old soldering iron tip is severely oxidized and turns black, you can use a steel foil to remove the surface oxide to expose the metallic luster, and then re-tin plating it before use.

The soldering iron requires a 220V AC power supply, and special attention should be paid to safety when using it. The following points should be carefully done:

It is best to use a three-pole plug for the soldering iron plug. Make sure the enclosure is properly grounded.

Before use, carefully check whether the power plug and power cord are damaged. And check whether the soldering iron tip is loose.

When using the soldering iron, do not hit it hard. Be careful not to fall. If there is too much solder on the soldering iron tip, wipe it off with a cloth. Do not throw it around to avoid burning others.

During the welding process, the soldering iron cannot be left lying around. When not soldering, it should be placed on the soldering iron stand. Note that the power cord cannot be placed on the soldering iron tip to prevent the insulation layer from being burned and causing an accident.

After use, the power supply should be cut off immediately and the power plug should be unplugged. After cooling, put the soldering iron back into the tool box.

2. Solder and flux

When welding, solder and flux are also needed.

(1) Solder: To weld electronic components, solder wire with a rosin core is generally used. This kind of solder wire has a lower melting point and contains rosin flux, making it extremely easy to use.

(2) Flux: Commonly used flux is rosin or rosin water (dissolve rosin in alcohol). Using flux can help remove oxides from the metal surface, facilitate soldering, and protect the soldering iron tip. Solder paste can also be used when soldering larger components or wires. However, it is corrosive to a certain extent, and the residue should be removed promptly after welding.

3. Auxiliary tools

To facilitate welding operations, needle-nose pliers, offset pliers, tweezers, and knives are often used as auxiliary tools. You should learn to use these tools correctly.

2. Pre-welding treatment

Before welding, pre-soldering treatment should be performed on the component pins or the soldering parts of the circuit board.

1. Remove the oxide layer from the welding part

Knives can be made from broken saw blades. Scrape off the oxide layer on the surface of the metal lead to reveal the metallic luster of the pin. The printed circuit board can be polished with fine gauze paper and then coated with a layer of rosin alcohol solution.

2. Tin plating of components

Tin the scraped leads. You can dip the lead in the rosin alcohol solution, press the hot soldering iron tip with tin on the lead, and turn the lead. This allows the leads to be evenly plated with a thin layer of tin. Before welding the wires, the insulation sheath should be stripped off, and then the above two treatments can be done before formal welding. If it is a wire with multiple strands of metal wire, it should be twisted together first after polishing, and then tinned.